Welcome to ModelEngineMaker !If you have problems registering or logging in, please use the contact menu option to request assistance.
the crankcase is ready for cleaning/soldering. kozo says "two or more heating/acid-cleaning steps will be required"does this mean i should only flux up / screw in place 2 of the bulkheads to for a first session, then acid clean again and flux up the remaining 2? i do have the higher temp black flux.thanks for all advice!edit - and oh yea, is this nozzle and mapp gas going to be enough "umph"?
edit - and oh yea, is this nozzle and mapp gas going to be enough "umph"?
Attached is a pic of my original Shay - JohnS.
https://www.riogrande.com/product/bronze-wire-solder-20-ga/132203 they have several products of this type,, the thin size works very nice and helps prevent to much solder on the work piece, depending on the color match, it makes to joints very hard to see. a ceramic soldering base helps keep your heat from being drawn away.. for most silver soldering I use mapp gas..
just like normal hard silver solder,, being in a fine wire helps with control.. another great item https://www.riogrande.com/product/knew-concepts-titanium-soldering-strip-set/110795